In this article, the first part of a two‐part study, we report the reaction path and microstructure evolution during the reactive hot isostatic pressing of Ti 3 SiC 2 , starting with titanium, SiC, and graphite powders. A series of interrupted hot isostatic press runs have been conducted as a function of temperature (1200°–1600°C) and time (0–24 h). Based on X‐ray diffractometry and scanning electron microscopy, at 1200°C, the intermediate phases are TiC x and Ti 5 Si 3 C x . Fully dense, essentially single‐phase samples are fabricated in the 1450°–1700°C temperature range. The time‐temperature processing envelope for fabricating microstructures with small (3–5 μm), large (∼200 μm), and duplex grains, in which large (100–200 μm) Ti 3 SiC 2 grains are embedded in a much finer matrix, is delineated. The microstructure evolution is, to a large extent, determined by (i) the presence of unreacted phases, mainly TiC x , which inhibits grain growth; (ii) a large anisotropy in growth rates along the c and a directions (at 1450°C, growth normal to the basal planes is about an order of magnitude smaller than that parallel to these planes; at 1600°C, the ratio is 4); and (iii) the impingement of grains. Ti 3 SiC 2 is thermally stable under vacuum and argon atmosphere at temperatures as high as 1600°C for as long as 24 h. The influence of grain size on the mechanical properties is discussed in the second part of this study.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
El‐Raghy et al. (1999) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: