Answers are grounded in this paper and cite their sources.
Single crystals of p‐Cu 2 S are obtained with a hole concentration of 7.4 × 10 19 cm −3 , a mobility of 25 cm 2 V −1 S −1 , and a thermoelectric power of 90 mV/deg. The electrical conductivity, thermoelectric power and Hall effect are measured between 20 and 600°C. A jump due to structural transformations is observed in the temperature dependence of these parameters at 125 and 480°C. The activation energy is found to have a value of 1.8 eV for the intrinsic range of the conductivity, the value found for the extrinsic range being 0.064 eV.
No takes yet. Share an insight, caveat, or question.
Abdullaev et al. (1968) studied this question.