The study of calcination treatment at 450°C on Ca-Mg-Al-hydrotalcite from brine water has been investigated. Characterization by XRD shows that Ca-Mg-Al hydrotalcite compound has found hydrotalcite phase and another phase such as Mg(OH)₂, Al(OH)₃ and CaCO₃. These results are confirmed by the presence of hydroxyl groups, M-O and M-OH groups (M is Mg, Ca and Al) at wavenumber region around 3464.35 cm⁻¹, 447.50 cm⁻¹ and 531.41 cm⁻¹. The calcination effect on Ca-Mg-Al hydrotalcite compounds at 450ºC being led to changes in structure become an metal oxide such as MgO, CaO, Al₂O₃, MgAl₂O₄ and CaCO₃. These results are confirmed from decreasing on the absorption peak of M-OH group at wavenumbers region around 531.41 cm⁻¹ and 786.99 cm⁻¹ and widening of the absorption region at 500-900 cm⁻¹. Consequently, the calcination treatment successfully increased the surface area of Ca-Mg-Al hydrotalcite compounds from 97.4 m²/g to 156.826 m²/g. Morphology of Ca-Mg-Al hydrotalcite changes the shape from a big to be small shape and the particle size distribution of 0-0.25 μm into 0-1 μm. Thermal analysis showed changes in the structure of hydrotalcite into oxide begins at a temperature of 265°C and started to become oxide completely after the temperature reaches 428°C.
No takes yet. Share an insight, caveat, or question.
Heraldy et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: