Platinum ultramicrodisk electrodes 0.8 μm in radius were constructed by anodic electropolishing of a platinum wire followed by sealing it with soft glass. Voltammograms for oxidation of [Mo(CN)8]4−, Fe2−, and [Fe(CN)6]4−, being of a sigmoidal form, were measured at these electrodes and microdisk electrodes with 7.5 μm in radius under the essentially steady-state condition. A voltammogram of Fe2+ at 7.5 μm electrode was drawn out, exhibiting a halfwave potential shifted from the formal potential. This trend was more distinctive for a wave at 0.8 μm electrode. Radii of the electrodes and diffusion coefficients of the electroactive species were determined consistently from the limiting currents. The conventional log-plot showed that electrode reactions of Fe2+ and [Fe(CN)6]4− were, respectively, totally irreversible and almost reversible at these electrodes. Application of the modified log-plot to the voltammograms yielded straight line, of which slope allowed us to evaluate the transfer coefficient and of which intercept gave values of the charge-transfer rate constant. Simulated voltammograms at these values were in good agreement with experimental ones.
No takes yet. Share an insight, caveat, or question.
Abe et al. (1988) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: