Answers are grounded in this paper and cite their sources.
Cellular polypropylene (PP) films were fluorinated under a high pressure of 13 bar of the F2/N2 mixture and were post-treated by nitrous oxide and isothermal crystallization. The fluorinated and post-treated PP films after being expanded and corona charged exhibit a significantly improved piezoelectric thermal stability. After annealing at 70 °C for 151 h or at 90 °C for 224 h, the piezoelectric d33 value of the fluorinated and post-treated piezoelectric sample still retains 58% or 45% of its initial d33 value, while the corresponding value of the virgin piezoelectric sample has decreased to 29% or 15% of the initial value. Chemical composition analysis of the cross section of the fluorinated and post-treated film by energy-dispersive x-ray spectroscopy indicates that the internal layers have been fluorinated, in spite of a lower degree of fluorination compared with the fluorinated surface layer. Short-circuit and open-circuit TSD current measurements reveal that the fluorinated internal layers, like the fluorinated surface layer, also have very deep charge traps, although there probably is a difference in density of the deep traps between them. The deeply trapped charge on the internal layers of the fluorinated and post-treated piezoelectric sample is responsible for its significantly improved piezoelectric thermal stability.
No takes yet. Share an insight, caveat, or question.
An et al. (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: