Answers are grounded in this paper and cite their sources.
Because the rate of anodic deposition for manganese oxide is much larger than that for nickel oxide, the nickel content of binary Mn-Ni oxide can be increased by using a relatively positive potential region and a high Ni 2 + / Mn 2 + ratio (10/1) in the deposition solution. The capacitive characteristics of this binary oxide in a mixed electrolyte consisting of 0.1 M Na 2 SO 4 with pH 10.1 adjusted by 0.01 M NaOH are much more ideal than that measured in 0.1 M Na 2 SO 4 . The effects of introducing Ni oxide into the MnO x matrix on the capacitive performance are systematically investigated. The nanostructure of this Mn-Ni oxide deposit is demonstrated from the scanning electron microscopic morphology.
No takes yet. Share an insight, caveat, or question.
Chen et al. (2003) studied this question.