Polyglycolide (PGA) is synthesized via ring‐opening polymerization (ROP) of diglycolide using the organocatalysts 1,8‐diazabicyclo[5.4.0]undec‐7‐ene (DBU), 1,5‐diazabicyclo[4.3.0]non‐5‐ene, or 1,5,7‐ triazabicyclo[4.4.0]dec‐5‐ene. ROP is carried out at low temperatures ranging from −20 to 50 °C without adding any alcohol as initiator. All polymers are fully soluble in hexafluoroisopropanol. At ambient temperature number average molecular weights up to 27 000 g mol −1 are obtained. With DBU the highest molecular weights and conversions are accessible at −20 °C. Melting temperature and glass transition temperature are independent of PGA molecular weight. Carrying out the reactions in the presence of polyethylene glycol serving as macroinitiator yields polymers with improved thermal stability and lowered melting temperatures.