Steady-state photoluminescence measurements performed on n-GaAs electrodes used in photoelectrochemical cells (PEC’s) employing a stabilizing, aqueous telluride electrolyte yield values for the electrode’s depletion width W and surface hole-capture velocity S. Between −1.0 V (a potential near short circuit) and −1.5 V vs an SCE reference electrode (a potential near open circuit at the photon flux of 1×1015 photons/s cm2 employed), the interface behaves ideally: virtually all of the applied potential appears in the semiconductor space-charge region. Over this potential regime S is determined to be constant to within 10% and has a value, using literature values for hole lifetime and diffusion length, of approximately 2×105 cm/s for n-GaAs electrodes having carrier concentrations of (1–4)×1017 cm−3. Similar values of S obtained in air and in the PEC suggest a common rate-limiting mechanism for hole consumption in the two media.
No takes yet. Share an insight, caveat, or question.
Burk et al. (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: