Answers are grounded in this paper and cite their sources.
Low pressure chemically vapor deposited polysilicon deposition was studied from 525 to 650°C. The silicon appears to be amorphous with a smooth surface up to 550°C and completely crystalline above 600°C. The transition region is found to be from 560 to 590°C. This transition is marked by sharp crystallographic and resistivity changes. The smooth surface morphology of the amorphous silicon is found to be preserved after doping and a 1000°C oxidation. The preservation of this smooth morphology is demonstrated to be due to the presence of a native oxide on the surface of the silicon upon exposure to atmosphere. However, an in situ anneal of amorphous silicon at 610°C results in large coarse crystals with rough surface morphology and disparate orientation. The smooth morphology of the 550°C silicon is found to be transmitted through subsequent polycide structure layers. The impact on device reliability is discussed. The amorphous silicon is found to have a higher plasma etch rate than the polysilicon.
No takes yet. Share an insight, caveat, or question.
Ibok et al. (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: