Calcium hydroxoaluminate hydrates were precipitated from different sodium hydroxoaluminate and hydroxoaluminate‐excess hydroxide solutions at ambient temperature (at C Al = 0.1 to 0.3 M and at XS OH/Al = 0 to above 8). The precipitations were monitored by potentiometric ( p H) measurements. Precipitate morphologies were examined by optical microscopy and precipitate compositions were determine by chemical analysis, infra‐red spectrophotometry and thermal analysis. Generally at OH/Al ratios of 4 to 4.5 (XS OH/Al = 1 to 1.5), the compound 2 CaO · · Al 2 O 3 · 8 H 2 O (C 2 AH 8 ) was precipitated with some aluminium hydroxide; then at OH/Al ratios of 5 to above 11 (XS OH/Al = 2 to above 8), the compound 2 CaO · Al 2 O 3 · 8 H 2 O was precipitated with increasing amounts of the compound 4 CaO · Al 2 O 3 · 13 H 2 O (C 4 AH 13 ).
No takes yet. Share an insight, caveat, or question.
Packter et al. (1983) studied this question.