We report a detailed investigation of the precipitation behavior of gold in float-zone silicon from a highly supersaturated solution. Nucleation, morphology, and crystallography as well as the decomposition of the solution were examined using high-resolution electron microscopy, selected area diffraction combined with tilting experiments, Hall-effect measurements, and energy dispersive x-ray spectroscopy. After in-diffusion of gold at 1275 ^∘{}C annealing experiments were performed at 850 ^∘{}C for durations ranging from 5 min up to 35 d. It is shown that gold precipitates in small spherical particles (diameter: 10--20 nm) consisting of a metastable gold silicide. By means of selected area diffraction combined with a special tilting procedure, the unit cell is proved to be orthorhombic with lattice parameters a=0.971 nm, b=0.768 nm, and c=0.703 nm. Systematic absence of reflections in several precipitate zone-axis patterns reveals the space group of the silicide to be Pnma or Pn2₁a. According to Hall-effect measurements the concentration of substitutional gold decreases to a few percent within 5 min annealing at 850 ^∘{}C. Only a part of it has precipitated in gold silicide particles, which are found at small extrinsic stacking faults. The stacking faults represent a density of self-interstitials Siᵢ of about 10¹⁸ cm^-3, which according to control experiments is about a factor of 50 above the equilibrium concentration of Siᵢ at 1274 ^∘{}C. As annealing proceeds the stacking faults disappear, and gold is finally found in spherical particles embedded stress-free into the silicon matrix.
No takes yet. Share an insight, caveat, or question.
Baumann et al. (1991) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: