This is the authors' abstract. We don't add key points for this paper.
We have examined the etch selectivity of homostructures of 1 μm of on both a nonintentionally doped (NID) substrate and a substrate. Samples were etched at 1.38 W/cm 2 in a 1:20 electrolyte over a bias range from −0.5 to +0.5 V. The selectivity of the structure is extremely high at ≥(15,000:1). The selectivity of the structure is significantly less, on the order of (30:1). The relative etch selectivity of the latter structure has a strong dependence on applied bias.