Answers are grounded in this paper and cite their sources.
The densities of undrawn and drawn nylon filaments (6‐6 Nylon) are found to be 1.1339 and 1.1384, respectively, at 25°C. Annealing either the drawn or undrawn forms to the highest temperature possible short of melting increases the room temperature density to 1.1564, the most rapid increase in density with temperatures annealing coming at 210°C. The temperature coefficient of the density as measured at room temperature is greater for the drawn form of the nylon than the undrawn after annealing has taken place. The density of nylon calculated by Bunn and Garner from x‐ray diagram data is 1.24, considerably higher than the highest value obtained by us on annealing, namely 1.156.