Answers are grounded in this paper and cite their sources.
Mixtures of copper and iron oxides are used as industrial catalysts for the water−gas shift (WGS, CO + H 2 O → H 2 + CO 2 ). In-situ time-resolved X-ray diffraction, X-ray absorption fine structure, and atomic pair distribution function analysis were used to study the reduction of CuFe 2 O 4 with CO and the behavior of CuFe 2 O 4 and Cu/Fe 2 O 3 catalysts under WGS reaction conditions. Metal↔oxygen↔metal interactions enhance the stability of Cu 2+ and Fe 3+ in the CuFe 2 O 4 lattice, and the mixed-metal oxide is much more difficult to reduce than CuO or Fe 2 O 3 . Furthermore, after heating mixtures of CuFe 2 O 4 /CuO in the presence of CO or CO/H 2 O, the cations of CuO migrate into octahedral sites of the CuFe 2 O 4 lattice at temperatures (200−250 °C) in which CuO is not stable. Above 250 °C, copper leaves the oxide, the occupancy of the octahedral sites in CuFe 2 O 4 decreases, and diffraction lines for metallic Cu appear. From 350 to 450 °C, there is a massive reduction of CuFe 2 O 4 with the formation of metallic Cu and Fe 3 O 4 . At this point, the sample becomes catalytically active for the production of H 2 from the reaction of H 2 O with CO. Neutral Cu 0 (i.e., no Cu 1+ or Cu 2+ cations) is the active species in the catalysts, but interactions with the oxide support cannot be neglected. These studies illustrate the importance of in situ characterization when dealing with mixed-metal oxide WGS catalysts.
No takes yet. Share an insight, caveat, or question.
Estrella et al. (2009) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: