Answers are grounded in this paper and cite their sources.
In this paper, (100-m) BaZrO3-mY2O3 (m = 0, 20, 25, 33, 50, 100) crucibles were prepared, respectively. Then, the effect of crucible composition on the interaction between crucibles and highly active titanium alloys (Ti2Ni) was investigated. The degree of the erosion resistance of crucibles was compared before and after melting as well as the contaminated extent of the alloys. The results show that the two-phase crucibles consisting of BaZr1−xYxO3−δ and Y2O3(ZrO2), could be prepared after adding Y2O3 into the BaZrO3 crucible. As the amount of Y2O3 addition in the crucible was increased, the erosion resistance of the crucible to the alloy melt was gradually improved. The two-phase crucible with 50 wt.% Y2O3 addition exhibited the best erosion resistance with a 7 μm thick erosion layer, which was at the same level compared to the pure Y2O3 crucible (6.5 μm). However, the inclusion contaminants caused by this two-phase crucible were smaller than those of the pure Y2O3 crucible. This study provided a theoretical basis for further research on the preparation of highly stable crucibles for melting highly active titanium alloys.
No takes yet. Share an insight, caveat, or question.
Feng et al. (2024) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: