Lanthanide (Eu and Nd)-doped hydrocalumite has been prepared by a coprecipitation method. All samples, with Eu 3+ and Nd 3+ contents up to 4% (molar ratio), show a single crystallographic phase, without segregation of secondary lanthanide-containing phases. Calcination affords lime and mayenite, with lanthanide cations embedded in the structure. The photoluminescence spectra of the noncalcined samples consist of Eu 3+ (in the visible region) and Nd 3+ (in the NIR) intra-4f transitions and a broad band ascribed to Al-related defects. The Eu 3+5 D 0 lifetime values and quantum efficiency of the Eu 3+ /Nd 3+ codoped hydrocalumite decrease ca. 10%, relative to the single doped material, suggesting that the Nd 3+ incorporation activates nonradiative channels for the 5 D 0 depopulation. High-temperature stable ceramic pigments, prepared from Eu 3+ and Nd 3+ doped hydrocalumite precursors, afford multiwavelength luminescent materials emitting in a large vis/NIR spectral region, with potential applications as barcodes and in broadband amplifiers. The emission spectra of the calcined samples give unequivocal evidence for the presence of two Eu 3+ local environments, attributed to Eu 3+ sites in CaO and mayenite. Upon calcination, the absolute emission quantum yield of the Eu 3+ -doped sample increases from less than 0.01 to 0.06.
No takes yet. Share an insight, caveat, or question.
Domínguez et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: