Helium-atom scattering has been used to study the facetting of an aluminum crystal that was cut at an angle of 10.0^∘{} from the (111) face to produce a (332) periodically stepped surface. After initial surface preparation of repeated sputtering and annealing cycles, the diffraction peak structures indicated strong facetting. Data collected for a wide range of initial He-atom wave vectors between 4.3 A^-1 (9.7 meV) and 12.5 A^-1 (81.8 meV) along the [1{} 1{}3] azimuth reveal well-formed (111), disordered (221), and a small proportion of (113) facets. The identification of facets is made relatively easy with He-atom scattering due to the large form factors for individual steps. From studies of the temperature dependence, three temperature ranges were identified. At the highest investigated surface temperatures (TAl>650 K), (111) and (221) facets build up and predominate. For intermediate temperatures (650 K>TAl>500 K) the macroscopic (332) face begins to form. At lower temperatures the surface is sufficiently immobile to inhibit a redistribution between facets. However, (221) facets do show a temperature-dependent roughness down to 300 K. The instantaneous long-range step distribution freezes in at TAl{≤}500 K.
No takes yet. Share an insight, caveat, or question.
Hinch et al. (1990) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: