Answers are grounded in this paper and cite their sources.
Mesoporous aluminosilicate AlSBA-15 was synthesized and adopted as a support for NiO with 3, 6 and 9 wt.% loadings. Characterization of various samples was performed through XRD, FTIR, DSC-TGA, TPR, SEM and TEM techniques. Textural and morphological characteristics were examined using N2 adsorption–desorption isotherms. Catalytic activities were measured in cumene cracking for parent AlSBA-15 and in n-hexane and toluene cracking and cyclohexane dehydrogenation for supported NiO samples. Uniformity of the ordered 2D-hexagonal structure of AlSBA-15 was evident even after loading with NiO. NiO and NiOOH phases could be detected particularly in the sample containing 9 wt.% NiO. TPR profile of solid loaded with 3 wt.% NiO sample showed negative peaks at 400 and 600 °C, related to hydrogen spillover on reduced sample. Selectivity towards n-hexane and toluene cracking increased with both temperature and metal oxide loading, achieving 100% at 350 °C. In cyclohexane dehydrogenation, the sample loaded with 3 wt.% NiO was the most active and selective one towards benzene formation.
No takes yet. Share an insight, caveat, or question.
Heba M. Gobara (2012) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: