In this paper, high-energy ball milling method was used to prepare LiFePO4/C precursor and high temperature solid phase method to prepare LiFePO4/C cathode material. The influence of mixing process on the electrical performance and synthesis temperature of LiFePO4/C cathode material was studied by changing the ball milling time.The ball milling time selected in this paper is 0, 0.5, 1, 1.5, 2 h, and XRD, SEM and particle size analysis are used to characterize the properties of LiFePO4/C powder. The research results show that the LiFePO4/C powder obtained under the ball milling time of 1 h has the smallest particle size and uniform distribution. The XRD results also show that the LiFePO4/C phase obtained under this condition has good purity and crystallinity.The electrical performance of the LiFePO4/C material prepared after high-energy ball milling are tested. The results show that the first discharge specific capacity at 0.2 C rate is 163.3 m·Ah/g, which is 19.7% higher than that of the non-ball milled sample.The TG-DTA curve results show that the reaction temperature of the sample after high-energy ball milling is 454 °C, and the mass loss ends at about 570 °C. Compared with the sample without ball milling, the reaction temperature is reduced by 60 °C.The results of this study show that the preparation of precursor by high-energy ball milling can effectively improve the electrical performance of LiFePO4/C materials and reduce the material synthesis temperature.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Cheng et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: