The first reduction reactions of solid SiO are reported. When SiO is heated with elemental magnesium, Mg2Si is formed at about 300 °C. The silicide disproportionates with excess SiO at about °C to give nanocrystalline silicon particles (crystalline diameter 11 nm) and MgO.