Answers are grounded in this paper and cite their sources.
Magnetostriction constants h 1 and h 2 of Pd-Co alloys containing 5∼60 at%Co have been measured in the temperature range between 77 K and 300 K. The values of h 1 and h 2 at 0 K determined by the extrapolation increase in magnitude with increasing Co concentration, and reach the maxima of about -3.1 ×10 -4 and -2.9 ×10 -4 at about 15 at%Co, respectively. With further increase of Co, h 1 decreases rapidly in magnitude and becomes positive above about 40 at%Co, while h 2 decreases gradually without change in sign.
No takes yet. Share an insight, caveat, or question.
Tokunaga et al. (1981) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: