We have measured the dependence of the transport critical current density on magnetic field and temperature of a high-Jc Bi-Sr-Ca-Cu-O/Ag tape sample. At low temperature, Jc>10⁴ A/cm² extending to high fields as previously reported by several groups. For T>20 K and with the applied field parallel to the c axis Jc declines precipitously with increasing field and temperature, reflecting the properties of intragranular pinning. The variation of Jc with the angle between B and the tape normal is consistent with a two-dimensional model of the vortex lattice. Independent determination of Jc by magnetic hysteresis measurement shows rough agreement with transport Jc's at low fields but falls below by a factor that increases with increasing field and temperature. This can be accounted for by a model for thermally activated flux motion.