Vacuum breakdown and field emission measurements have been obtained for W and Mo wire cathodes as a function of annealing temperature using a variety of cylindrical anodes (Cu, W, Al and Mo). The cathode surface structure was investigated using a scanning electron microscope. These observations are shown to indicate that initial surface protrusions capable of giving reproducible Fowler-Nordheim plots consist mainly of impurities. Pure metallic protrusions are only formed after breakdown following high-temperature cathode annealing. Breakdown after the highest temperature annealing treatment appears not to be field emission dominated.