This is the authors' abstract. We don't add key points for this paper.
Improved overall critical current densities Jc’s were achieved with powder metallurgy processed Nb-A1 which combined reduced powder sizes and increased nominal areal reductions R. Increased Jc values were obtained for a variety of different heat treatments. For a Nb-8 wt. % A1 wire with R=3.4×105 a very short treatment at 1100 °C followed by a 750 °C treatment gave (at 4.2 K)Jc>104 A/cm2 at 19 T; a 900 °C treatment followed by a 750 °C treatment gave Jc=104 A/cm2 at 18 T and, at 2 K, Jc was greater than 104 A/cm2 at 20 T; and a treatment of 800 °C for 8 h gave (at 4.2 K)Jc=104 A/cm2 at 17.5 T.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Thieme et al. (1984) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: