Answers are grounded in this paper and cite their sources.
We report the first p-n junction delineation and diffusion study in a ternary chalcopyrite-type semiconductor. p-n junctions were formed in Zn- or Cd-plated p-CuInSe2 by 5-min anneals at 200–450 °C. By means of angle lapping and staining techniques, junction depths xj varying from ∼1 μm to ∼130 μm were determined. These measurements yield the relationship lnxj (μm) =14.31−6900/T (K). The interdiffusion coefficient derived from xj is D (cm2/sec) =164 exp[−1.19 (eV)/kT]. The large preexponential term indicates concentrations or mobilities of point defects substantially above those of the related II-VI compounds.
No takes yet. Share an insight, caveat, or question.
Tell et al. (1976) studied this question.