Measurements of the temperature dependence of the longitudinal and shear ultrasonic attenuation from 5 to 50 Mc/sec were made in SiO2, GeO2, B2O3, and As2O3 glass. In each case a relaxation loss with a distribution of relaxation times was found. The median activation energy of the relaxation process is about 500 cal/mole in SiO2, 2500 cal/mole in GeO2, 5400 cal/mole in As2O3, and 6300 cal/mole in B2O3. The results are interpreted in terms of a two-bond-length model of glass where the relaxation loss is associated with bridging oxygen atoms which have two stress-sensitive equivalent equilibrium positions. A relationship between the relaxation loss mechanism and the viscosity of these glasses is assumed in this study. A calculation of the activation energies based upon this assumption agrees well with the values determined experimentally.
No takes yet. Share an insight, caveat, or question.
Strakna et al. (1964) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: