This is the authors' abstract. We don't add key points for this paper.
The complete set of electroelastic constants of a tetragonal lead titanate zirconate ceramic (PZT-5A) is shown as function of the invariant coupling factor ki3 (and, thus, as function of the thoroughness of poling). Interrelations among the important piezoelectric-coupling factors (k33, k31, kp, kt, ki1 = k15, and ki3) are also shown. Most measurements were repeated on a rhombohedral lead titanate zirconate ceramic {Pb0.9875Nb0.025(Zr0.65Ti0.35)0.975O3}. With the rhombohedral material, anisotropies increase throughout the entire range of ki3; but, with PZT-5A, anisotropies increase sharply only at the highest values of ki3 (range ∼0.6 to 0.75). Anisotropies of the elastic constants are much greater at constant D than at constant E. It is demonstrated that changes inelastic and dielectric constants near saturation are relatively severe, even with small changes in the coupling factors.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
D. Berlincourt (1964) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: