SIPOS (semi‐insulating polycrystalline silicon) films with 40 atomic percent oxygen have been studied with Auger electron spectroscopy (AES) and photoelectron spectroscopy (PES). The comparison of the Si LVV Auger spectra with the Si 2p lines suggests that the as‐grown SIPOS film contains large amounts of SiO x ( x < 2 ) as well as SiO 2 . Annealing at 1100°C causes crystal growth of Si and the change of SiO x towards SiO 2 . An additional peak at 83 eV is found in the Si LVV Auger spectra, which has been reported to exist at the Si ‐ SiO 2 interface, and can be attributed to SiO .