A biodegradable polymer coated with a bone-like apatite layer on its surface is useful as a scaffold for bone tissue regeneration. In this work, a poly(epsilon-caprolactone) (PCL) surface was modified by an O2 plasma surface treatment to form oxygen-containing functional groups. The plasma-treated samples were subsequently dipped alternately in an alcoholic solution containing calcium ions and one containing phosphate ions to deposit apatite precursors on the surface. The surface-modified PCL samples formed a dense and uniform surface bone-like apatite layer after immersion for 24 h in a simulated body fluid with ion concentrations approximately equal to those of human blood plasma. This surface-modification process is applicable to two-dimensional PCL plates and three-dimensional PCL meshes. In the resulting apatite-PCL composite, the apatite layer strongly adhered to the PCL surface and remained intact after a tape-detachment test. Therefore, this type of composite material will be a useful scaffold for bone tissue engineering.
No takes yet. Share an insight, caveat, or question.
Oyane et al. (2005) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: