The average grain size of ZrO 2 (+Y, o,) materials sintered at 1400°C was observed to depend significantly on the Y 2 O 3 content. The average grain size decreased by a factor of 4 to 5 for Y 2 O 3 contents between 0.8 and 1.4 mol% and increased at Y 2 O 3 contents of 6.6 mol%. Grain growth control by a second phase is the concept used to interpret these data; compositions with a small grain size lie within the two‐phase tetragonal + cubic phase field, and the size of the tetragonal grains is believed to be controlled by the cubic grains. This interpretation suggests that the Y 2 O 3 ‐rich boundary of the two‐phase field lies between 0.8 and 1.4 mol% Y 2 O 3 . Transformation toughened materials fabricated in this binary system must have a composition that lies within the two‐phase field to obtain the small grain size required, in part, to retain the tetragonal toughening agent.
No takes yet. Share an insight, caveat, or question.
F. F. Lange (1986) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: