Magnetization measurements are reported for homogeneous materials Sm 0.167 Co 0.833-x Al x both in bulk and 'oriented powder' form over a temperature range of 1.6-280K with fields up to 45 kOe. At cryogenic temperatures (4.2K) outstanding magnetic hardness is found in both the Al rich powder and the bulk specimen, with coercive forces, H c , of order 40-50 kOe. This magnetic hardness decays with temperature according to a Curie type law. It is inferred from these findings that the domain wall energy increases strongly on Al substitution. Moreover, when Al is substituted for Co, the predominant mode of domain reversal changes at cryogenic temperatures from a mechanism involving domain wall nucleation to one of domain wall pinning. The mechanism of magnetization in highly energetic domain wall materials is shown to reflect in a delicate way details of structure on an atomic scale. Some preliminary results are presented for alloys Sm 2 Co 17 and Sm 2 Co 7 with Al substitution for Co. An exploratory effort at coating SmCo 5 powders with its Al substituted derivatives has been carried out via sintering with either Al or Sm-Al compounds. The potential for applications of Al derivatives of SmCo 5 in the fabrication process of permanent magnets is discussed.
No takes yet. Share an insight, caveat, or question.
H. Óesterreicher (1975) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: