The remanent magnetization of acicular γ−Fe2O3 particles partially converted to hematite by heating in air was measured after saturation and ac demagnetization using a vibrating-sample magnetometer. It is possible that commercial γ−Fe2O3 recording tapes could undergo this partial conversion which may result in a deterioration of their magnetic properties. The complete composition range from pure γ Fe2O3 to hematite was studied. The composition was determined by interpolation of the saturation magnetization of the sample and of the values for pure γ Fe2O3 and hematite. The remanent magnetization increases as a function of hematite composition. At 90% hematite there is a peak in the remanent magnetization which is a factor of 2 greater than the remanence of the two components. The coercivity was approximately constant, 320 Oe, as a function of composition except that pure hematite had a value of 635 Oe. Partially converted particles were examined using dark-field electron microscopy to indicate the method of conversion.
No takes yet. Share an insight, caveat, or question.
Gustard et al. (1966) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: