This is the authors' abstract. We don't add key points for this paper.
Glass transition temperatures of a very wide molecular-weight range of ethylene oxide polymers were measured by mechanical loss and by broadline NMR. Starting at about −95°C for ethylene glycol, the glass transition rises to a maximum of −17° for molecular weight 6000 and then drops off to −53° for polymers with molecular weights greater than 200 000. This unusual behavior is probably caused by the high crystallinity of the intermediate molecular-weight polymers.