We have investigated the physical microstructure and Lorentz magnetic structure of in-situ ion beam sputtered and RF sputtered amorphous Gd-Fe alloy thin films. Auger electron spectroscopy was used to determine the composition profile and thickness of the films. Films with 18 to 30 at.% Gd were deposited onto amorphous carbon substrates up to 500 Å inside a modified RCA-EMU4 electron microscope. Two diffused electron diffraction halos were observed indicating amorphous phase separation. Using high-resolution dark-field microscopy with a JEOL (JEM-100C) electron microscope, we observed coherent scattering regions of approximately 8–20 Å diameter. In conclusion, amorphous Gd-Fe alloy films exhibit amorphous phase separation/quasi-amorphous structure, in-plane magnetization ripple and crosstie walls, and stress-induced anisotropy.