Iron‐tungsten alloys have been electrodeposited from the ferrous ammonium sulfate iron plating bath which was modified by the addition of small amounts of sodium tungstate. Alloy composition and cathode current efficiencies were studied at various current densities, bath pH's and bath temperatures. The tungsten content of the alloy was found to increase somewhat with: (a) increase in tungsten content of the bath; (b) decrease of cathode current density; (c) increase of bath temperature; and (d) decrease of bath pH. An increase of tungsten concentration in the bath was found to decrease the current efficiency of alloy deposition. The most satisfactory alloy deposit was obtained from a bath containing 1 to 2 g./L. of added tungsten. A rather high current density, a bath pH of 2, and a bath temperature of 75° C. were found to be the best conditions of electrolysis. It is suggested that reduction of tungstate ion at the cathode involves reduction by atomic hydrogen and/or by “unstable, active” iron.
No takes yet. Share an insight, caveat, or question.
Holt et al. (1942) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: