Answers are grounded in this paper and cite their sources.
In order to fabricate dense ZrO2-Al2O3 ceramics by pressure-less sintering, three kinds of granules of calcined neutralization co-precipitated 75 mol% ZrO2(2.0 mol%Y2O3)-25 mol%Al2O3 powders added with a small amount of cellulose nanofiber (CNF), i.e., (2, 2, 6, 6-tetramethylpiperidine 1-oxyl)-oxidized (TEMPO) CNF, non-oxidized CNF and polyvinyl alcohol (PVA) were prepared and compacted. Then, they were sintered at 1523 K for 8.64·104 s in air. The granules prepared via the addition of 0.15 mass% TEMPO-CNF revealed a low relative density Dr for powder compacts (43.0%), however, they showed the highest Dr (99.8%) of sintered ceramics with the excellent mechanical properties, i.e., Vickers hardness Hv of 15.4 GPa, fracture toughness KIC of 18.2 MPa·m1/2 and bending strength σb of 882 MPa. These properties are almost the same as those fabricated by pulsed electric-current pressure sintering (PECPS). This might be explained in terms of i) the charged 1st particles induced by TEMPO-oxidized CNF addition could form the nano meter-gap between the primary particles in the granules, and then ii) this nano meter-gap could suppress the particle-sintering at relatively low temperatures, and then much densification at high temperatures could be achieved.
No takes yet. Share an insight, caveat, or question.
Yoshida et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: