Answers are grounded in this paper and cite their sources.
The microstructure and phase composition of the high-content Al 2 O 3 -Y 2 O 3 -doped spark plasma-sintered silicon nitride were investigated. Fully dense silicon nitride ceramics with a typical α-Si 3 N 4 equiaxed structure with average grain size from 200 to 530 nm, high elastic modulus of 288 GPa, and high hardness of 2038 HV were spark plasma sintered (SPSed) at 1550 °C. Silicon nitride with elongated β-Si 3 N 4 grains, higher hardness of 1800 HV, density of 3.25 g/cm 3 , and Young’s modulus 300 GPa SPSed at 1650 °C was also reviewed.
No takes yet. Share an insight, caveat, or question.
Lukianova et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: