In the conventional high‐temperature thermal oxidation and rapid thermal oxidation processes used to fabricate commercial SiO 2 /Si structures at ∼850–1050°C, the SiO 2 /Si interface and the bulk oxide are formed at the same time . We have developed a low‐temperature process for the formation of SiO 2 /Si structures at 200–300°C that separately controls and optimizes the properties of the SiO 2 /Si interface and the bulk SiO 2 . This has been accomplished by separating interface formation by plasma‐associated oxidation from bulk oxide plasma‐assisted deposition . The oxidation step (i) removes residual C contamination from the Si surface, (ii) prevents N incorporation at the interface from the O atom source gas N 2 O and (iii) forms an oxide layer ∼0.6 nm thick and an SiO 2 /Si interface with a trap density, D it ≈(1–4) × 10 10 cm −2 eV −1 . This type of process has also been extended to the deposition of multilayer oxide–nitride–oxide dielectrics.
No takes yet. Share an insight, caveat, or question.
G. Lucovsky (1993) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: