Co/Pt superlattices with an ultra-thin amorphous Ta seed layer on a Ni/sub 45/Fe/sub 55/ underlayer were fabricated for double-layer perpendicular magnetic recording media using a special hard disk sputtering system with a triple-target DC magnetron cathode (Triatron). A 2.5 nm thick Ta seed layer was found to improve the crystalline structure and increase the coercivity of the Co/Pt superlattices from 1.13 to 2.17 kOe. A 2.5 nm Ta layer on a 200 nm thick magnetically soft NiFe underlayer was found to further increase the coercivity from 2.25 to 5 kOe. In addition, the sheared slope of the sides of hysteresis loop of Co/Pt superlattices was significantly improved from about 5 Gauss/Oe (with only a 2.5 nm Ta seed layer) to about 1.1 Gauss/Oe (with both a 2.5 nm Ta seed layer and a 200 nm NiFe underlayer).
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Peng et al. (2000) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: