The results of a neutron-diffraction study of the magnetic structure properties of the Tb-Sc alloy system are reported. Five binary alloys with Tb content from 90 at. % to 25 at. % have been examined by powder techniques from 300°K down to liquid-helium temperatures to determine the magnetic ordering temperatures and the magnetic structures. The dilution by Sc causes the spiral magnetic phase of Tb to remain stable over a temperature interval larger than in the pure metal. This effect is the same general behavior as that found in the Tb-Y system previously reported. However, the Néel points of the Tb-Sc alloys fall well below those found for Tb-Y and the initial turn angles are smaller in this system. TN falls more rapidly for Tb-Sc alloys than for Tb-Y alloys as a function of the effective spin variable x=c(g−1)2J(J+1), where c is the atomic percent of Tb, and reaches 0°K at x about 2.5. The 25% Tb alloy shows no visible magnetic order down to 1.3°K in contrast to the Tb-Y system where magnetic order was observed with as little as 5 at. % Tb. The universal curve of TN vs x previously found for rare-earth alloys is not obeyed in the Tb-Sc system.
No takes yet. Share an insight, caveat, or question.
Child et al. (1966) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: