Answers are grounded in this paper and cite their sources.
The plastic properties of calcium fluoride single crystals tested in compression were investigated in the temperature range 25° to 1000°C. Above 400° C., the crystals showed appreciable ductility. The critical resolved shear stress, t, decreased with absolute temperature, T , according to the equation t = t 0 e +K/T . The rate of work‐hardening decreased rapidly as the temperature increased but retained a relatively high value even as the melting point was approached. Air‐annealed crystals were harder than as‐cleaved crystals. Crystals with a (111) plane normal to the applied stress hardened less rapidly than crystals with a (110) plane normal to the applied stress. The dislocation density increased linearly with strain. (100), (110), and (111) fractures were observed.
No takes yet. Share an insight, caveat, or question.
W. L. Phillips (1961) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: