Shear data in the temperature range from −145 °C to the flow zone are presented for the poly( n -alkyl methacrylate)s from methyl ( C = 1) to lauryl ( C = 12). Three qualitatively different glass transitions are observed in the shear curves at 10 rad/s: (i) the conventional α process in the C < 5 members, (ii) the high temperature a process in the C > 5 members, and (iii) an additional polyethylene-like glass transition, α PE, in the C ≥ 3 members. All three processes depend systematically on side chain length. Two alternative empirical pictures for the coexistence of two glass transitions are discussed: (a) a static nanophase separation between main chains and side chains and (b) a dynamic heterogeneity with two different time and length scales.