Answers are grounded in this paper and cite their sources.
Simultaneous measurements of the length change and resistivity of high-purity germanium single crystals were made upon irradiation and annealing. The specimens were initially irradiated at 25^∘{}K with deuterons of average energy 10.2 Mev to an integrated flux of 6.2×{}10¹⁶ deuterons/cm² and annealed to room temperature. The specimens were then irradiated at 85^∘{}K to an additional flux of 9.2×{}10¹⁶ deuterons/cm² and annealed to 364^∘{}K. The specific length expansion for both bombardments was ΔLL=(1.5±0.3)×10^-21/(deuteron/cm²). The annealing after both irradiations showed a gradual recovery of the expansion which was observable only after warming to above 200^∘{}K. The precise determination of the onset of annealing was limited by the accuracy of the expansion measurements ({~}20%). Recovery was {~}50% complete by 300^∘{}K and {~}85% complete by 360^∘{}K. The resistivity measurements agreed generally with previous results. A large increase in resistivity occurred during the low-temperature bombardments. The specimens became p-type after bombardment and annealing. On the first warmup after the bombardment at 25^∘{}K the resistivity decreased irreversibly by a factor of 10⁶ between 65^∘{}K and 300^∘{}K with a large part of the decrease coming apparently between 150^∘{}K and 225^∘{}K. On the warmup from the second bombardment at 85^∘{}K an irreversible resistivity increase occurred on warming to 140^∘{}K. The resistivity then decreased irreversibly by a factor of 10³ between 150^∘{}K and 200^∘{}K. Extensive resistivity annealing, therefore, occurred in an earlier stage of the recovery process than did the experimentally observable length change annealing.
No takes yet. Share an insight, caveat, or question.
Vook et al. (1959) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: