In this study, two hydrogen sensors with Pd/SiO2/Si and Ni/SiO2/Si structures have been fabricated. Palladium nanoparticles are synthesized and then deposited on the oxide surface using spin coating. Capacitance–voltage curves for the Pd/SiO2/Si sensor at room temperature and for the Ni/SiO2/Si sensor at 140[Formula: see text]C in pure nitrogen and 1% H2–N2 mixture are described. The time required for reaching 90% of the steady-state signal magnitude ([Formula: see text]) for Pd/SiO2/Si capacitor was 1.4[Formula: see text]s and for Ni/SiO2/Si capacitor was 90 s. The time interval for recovery from 90% to 10% of steady-state signal magnitude ([Formula: see text] for Pd/SiO2/Si capacitor was 14[Formula: see text]s and for Ni/SiO2/Si capacitor was 40[Formula: see text]min. For the Pd/SiO2/Si capacitor, the response is 88% and for Ni/SiO2/Si capacitor the response is 29%. Comparison of Pd nanoparticles capacitive- and resistance-based sensors shows that the metal-oxide-semiconductor capacitive is faster and more sensitive than the resistance-based hydrogen gas sensors.
No takes yet. Share an insight, caveat, or question.
Pour et al. (2017) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: