Answers are grounded in this paper and cite their sources.
High-intensity ultrasonication was demonstrated to be facile and efficient for the preparation of water-dispersible poly(vinyl alcohol) functionalized vapor-grown carbon fibres (f-VGCFs). In contrast to multiwalled carbon nanotubes, VGCFs are mechanically strong and not observably shortened or damaged by ultrasonication. Fourier transform infrared spectroscopy, X-ray photoelectron spectroscopy and transmission electron microscopy show that the surface of f-VGCFs is decorated with a thin layer of PVA, imparting good dispersibility and suspending stability in water. High-strength PVA–f-VGCF composite films were then successfully obtained by the green and low-cost water casting method, which is totally free of organic solvents. The tensile strength and Young's modulus of the composite films filled with 5 wt% f-VGCFs are remarkably increased to 177.5 ± 9.8 MPa and 4.6 ± 0.4 GPa, respectively, which are about 45.0% and 53.3% higher than those of neat PVA. After being stretched by 5 times their length, the tensile strength and Young's modulus are increased to 681.0 ± 4.3 MPa and 12.1 ± 0.6 GPa, which are 58.8% and 49.4% higher than those of neat PVA stretched by 5 times their length, respectively. The uniform dispersion of f-VGCFs and the effective load transfer between the fillers and the matrix are responsible for the greatly improved mechanical properties.
No takes yet. Share an insight, caveat, or question.
Sun et al. (2013) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: