The range of solid solution has been investigated in alloys of PbTe-SnSe, PbTe-GeSe and SnTe-GeSe. The solubilities of SnSe and GeSe in PbTe were found to be limited at about 70 mol.% SnSe and 35 mol.% GeSe respectively. The lattice parameters of the alloys decrease linearly with concentration: for SnSe in PbTe, a 0 = 6.459 - 0.455 X Å and for GeSe in PbTe, a 0 = 6.459 - 0.745 X Å where X is the molar fraction of SnSe and GeSe respectively. The solubility of GeSe in SnTe was found to be limited at about 40 mol.% GeSe and the lattice parameter to decrease with GeSe content as a 0 = 6.303 - 0.55 X Å. Measurements of the variation of the optical energy gap have also been made for two of these alloys: E g increases with composition in PbTe-GeSe but decreases with composition in PbTe-SnSe.