This is the authors' abstract. We don't add key points for this paper.
High coercivity B-N-doped MnAl alloys were prepared by the traditional induction melting, high temperature homogenization, water-quenching, post-annealing, and severe plastic deformation process. The massive phase transformation of the ε→τ in the B-N-doped ε-MnAl occurs at the temperatures above 680 K and accomplishes at 760 K, both of which are slightly higher than those of the ε-MnAl without elemental doping. The Currie point of the B-N-doped τ-MnAl is measured to be 620 K, which is lower than that of the doping-free τ-MnAl. High-pressure torsion was employed to decrease the crystal size and increase the coercivity of samples. A coercivity up to 0.54 T was achieved in the B/N doped MnAl bulk sample after severe plastic deformation under 6 GPa. The aging processing on the severely deformed samples enhances the remanent magnetization significantly and decreases the coercivity slightly. Our work shows that the high-pressure torsion process is effective in developing coercivity in MnAl-based bulk magnet.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Si et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: