Nanometer thick layers of Mg metal vapor deposited onto a polycrystalline gold substrate at 22 K with and without O 2 multilayers were examined after annealing. Auger electron spectroscopy and temperature-programmed desorption of N 2 were used to determine the Mg oxidation state and the surface area of the deposits immediately after deposition at 22 K, and following annealing. Deposited on 20 layers of O 2, Mg oxidizes and forms an MgO film having a high surface area (∼700 m 2 /g). The surface area decreases upon annealing, approaching that of a well-ordered MgO(100) surface by 500 K. On thinner O 2 multilayers, both oxidized and metallic Mg are observed at 22 K. Mild thermal annealing (200−400 K) results in transport of the excess metallic Mg to, and alloy formation with, the underlying Au substrate. MgO films annealed to 1000 K display a narrow distribution of N 2 binding sites, similar to well-ordered MgO(100). The film sublimes above 1000 K when heated.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2004) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: