Silicon on sapphire wafer pairs are formed by direct wafer bonding of 3-in. silicon and sapphire wafers. Subsequent annealing commonly used to increase the bond energy imposes serious thermomechanical strain. The corresponding bending, recorded in situ as a function of temperature, reveals relaxations by de- and rebonding until the silicon wafer cracks into small fragments that mostly remain bonded. After further annealing up to 800 °C and cooling to room temperature, a strong curvature of the fragments indicates a frozen-in high temperature bond state with elastic energies around 100 J/m2. Cross-sectional transmission electron microscopy of the interface reveals an amorphous intermediate layer the thickness of which considerably increases with increasing the oxygen partial pressure during annealing.