Answers are grounded in this paper and cite their sources.
Various wire samples consisting of 19-Nb3Sn filaments in a normal metal matrix were made by heat treating composite wires of 19-Nb, Nb-0.5 wt% Zr, Nb-0.75 wt% Zr, and Nb-2.5 wt% Zr filaments embedded in a Cu-10 wt% Sn matrix. The Nb-0.75 wt% Zr rod contained the precipitate ZrO2, while the Zr in the remaining Nb rods was in solid solution. The over-all size of the composite was 2.5×10−2 cm and each filament was approximately 2.5×10−3 cm in diameter. The critical current density Jc at 4.2 °K was measured at 40 and 100 kG for a variety of heat treatments. It was found that the critical current density was a strong function of the thickness of the Nb3Sn layers formed during heat treatment. This dependence of Jc on the thickness d could be approximately represented by the expression Jc(d)≃J0 exp (−nd), where J0 is the extrapolated zero thickness critical current density. J0 was found to be approximately 2.4×106 A/cm2 at 40 kG for the Nb3Sn formed from pure Nb, 1.2×106 A/cm2 for Nb doped with solid-solution additions of Zr, and 9.5×105 A/cm2 for that formed from Nb doped with ZrO2. The exponent n falls in the range 0.52–0.67 (μm)−1 for pure Nb3Sn depending on heat treatment temperature, 0.154–0.287 (μm)−1 for Nb doped with solid-solution additions of Zr, and only 0.11 (μm)−1 for the Nb3Sn composite wire containing ZrO2. The magnetic field dependence of Jc for some of the composites was also measured to 150 kG.
No takes yet. Share an insight, caveat, or question.
Suenaga et al. (1974) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: